EN-2002-016
Reference | Edition | Title / Details |
ASD-STAN prEN 2172-002 | Heat resisting steel FE-PA92-HT – Rm > or= 900 MPa – Forgings |
Heat resisting steel FE-PA92-HT – Rm > or= 900 MPa – Forgings
pren-2172-002 This standard is available only on request – please Click here to Email for a price |
ASD-STAN prEN 3247 P2 | Pipe coupling 8°30′ in titanium alloy – Unions, bulkhead, welded |
Pipe coupling 8°30′ in titanium alloy – Unions, bulkhead, welded |
ASD-STAN prEN 2631-001 | Aluminium alloy 7075-T6511 – Bar and section – 1,2 ≤ (a or D) ≤ 125 mm – With peripheral coarse grain control |
Aluminium alloy 7075-T6511 – Bar and section – 1,2 ≤ (a or D) ≤ 125 mm – With peripheral coarse grain control |
ASD-STAN prEN 2198-001 | Heat resisting nickel base alloy Ni-P103-HT – Solution treated and precipitation treated – Precision castings |
Heat resisting nickel base alloy Ni-P103-HT – Solution treated and precipitation treated – Precision castings |
ASD-STAN prEN 3128 | Number reserved for C5 |
Number reserved for C5 |